Geometrical Boundary
Geometrical proportions of blind holes dictate the flow behavior of plating chemistry during the metalization phase of high-density interconnect board fabrication. For aspect ratio microvias, this value represents the depth of the laser-drilled hole divided by its starting diameter at the outer copper foil. When this ratio exceeds a critical threshold, the flow of liquid acid copper plating solution becomes restricted.
Inadequate replenishment hinders the transport of copper ions to prevent incomplete filling.
Plating Performance
Deposition uniformity depends on the transport of copper ions through the cavity. For aspect ratio microvias, a value below one to one allows standard pulse plating to balance the copper thickness. When the ratio increases, the risk of early pinching grows.
Reliability Consequence
Thermal stress testing reveals the structural integrity of the copper joint at the inner target pad. Inadequately proportioned aspect ratio microvias often result in thin copper layers that fail IPC-6012 Class 3 requirements during solder floating or convective reflow simulation. The resulting separation between the plated copper and the target pad creates intermittent open circuits that escape early optical inspection.
Continuous cross-sectional monitoring ensures that drilling and plating processes remain within established limits to prevent these defects. Modern designs limit these geometry choices to prevent long-term field failures from microcracking under thermal expansion.