Intermetallic Growth
Solid-state interconnections establish electrical paths between semiconductor die pads and leadframe terminals through micro-welding techniques. Micro-wire interconnections fabricated as copper wire bonds deliver high thermal conductivity and reduced electrical resistance compared to traditional gold alternatives. Oxidation resistance requires forming gas shielding during thermosonic ball formation.
Slow intermetallic compound growth rates at the aluminum pad interface reduce Kirkendall voiding during thermal aging.
Work Hardening
High yield strength inherent to copper requires elevated ultrasonic energy and bonding force during ball attachment. Thermosonic bonders attach copper wire bonds by applying mechanical pressure alongside high-frequency vibrations to displace pad aluminum oxide. Rigid mechanical properties increase the risk of substrate cratering beneath bond pads during ultrasonic energy transfer.
Process windows must balance scrub power against pad metallization thickness to prevent micro-fracturing of underlying dielectric layers. Flame-off systems flood the wire tip with ninety-five percent nitrogen and five percent hydrogen gas to form uniform unoxidized free air balls before capillary contact. Wire stitch bonds onto silver or palladium plated leadframes require tight mechanical control to avoid heel cracking caused by local work hardening.
Extended high-temperature exposure forms cu9al4 intermetallic phases that alter electrical conductivity at elevated junction temperatures.
Shear Testing
Mechanical destruction tests measure ball shear force and wire pull strength to verify bond integrity. Standard IPC and MIL-STD tests specify minimum ball shear resistance in grams per square mil of bond area. Shear failure modes that sheer pad metallization away from silicon substrate indicate improper capillary geometry or excessive bonding force.