Component Repair
Specialized removal and replacement procedures for fine-pitch ball grid arrays address defects like solder bridging or open joints on high-density assemblies. Precision alignment is required. Performing micro bga rework requires high-magnification optics and precision motion control to align parts with ball diameters as small as 0.2 millimeters.
The process involves desoldering the faulty chip, cleaning the pads on the board, applying new flux, and placing a new component with fresh solder spheres. Success depends on maintaining a thermal profile that mimics the original production run to ensure long-term reliability.
Tooling Requirement
Vacuum pick-up tools and split-prism imaging systems enable the technician to see the pads and the balls simultaneously for exact placement. Because the hidden nature of the joints prevents visual inspection, x-ray imaging is the only way to confirm a successful micro bga rework. Heat management is particularly difficult because the small mass of the chip makes it prone to rapid overheating.
Nitrogen shielding is often used to prevent pad oxidation during the multiple heat cycles.
Site Preparation
Removing residual solder from the board pads must be done with a non-contact system or specialized copper braid. Any damage to the solder mask or laminate at this stage renders the board scrap.