Roughness Measurement
Surface topography of copper foil determines both the mechanical bond with the dielectric resin and the signal propagation characteristics of high-frequency transmission lines. Measuring the profile height provides a quantified value of the vertical distance between the highest peak and the lowest valley on the copper surface. Lamination specifications require this value to be kept within tight bounds to ensure reliable manufacturing.
Trace adhesion suffers if the surface is too smooth.
Foil Adhesion
Foil manufacturing involves chemical treatments that deposit copper nodules to increase the bonding surface area. Managing the profile height is a trade-off because higher roughness increases the mechanical peel strength of the laminate but degrades signal integrity at microwave frequencies. High-frequency digital circuit boards require very low profile foils to minimize signal attenuation.
The lamination process must balance these mechanical and electrical needs to prevent delamination during subsequent thermal reflow cycles. Vacuum baking and cleanroom storage are used to prevent oxidation of these micro-structured surfaces before lamination.
Electrical Consequence
High-speed traces running on high-roughness foils experience severe skin effect losses at frequencies above five gigahertz. The signal current is forced to travel along the contoured surface, increasing the effective line length and resistance. Designers select low-profile foils to bypass this issue.