Fabric Specification
Mechanical spreading processes flatten glass yarn bundles to eliminate windows between intersecting fibers in thin electronic laminates. Fabric processed under 3313 mechanical spread exhibits broad, flat glass ribbons that replace conventional twisted circular yarns.
Weave Uniformity
High-pressure water jets or mechanical rollers expand the individual glass filaments outward after weaving. Standard 3313 glass fabric features a loose weave with open spaces between warp and weft threads, but 3313 mechanical spread forces those filaments into a continuous sheet profile. Eliminating open windows prevents pure resin pockets from forming in prepreg plies.
Microsection analysis confirms a reduction in localized dielectric variance across signal routing channels.
Impedance Stability
Transmission lines running over glass-reinforced substrates suffer from phase jitter when signal paths alternate between high-dielectric glass bundles and low-dielectric resin pockets. Expanding the 3313 yarn bundles distributes glass mass evenly across the substrate plane, maintaining a stable effective dielectric constant beneath narrow trace geometries. Differential signals propagating across the laminate maintain consistent propagation delays across both legs of a differential pair.
Circuit boards fabricated with unspread 3313 glass demonstrate localized impedance variations up to six ohms, whereas 3313 mechanical spread restricts impedance deviations to within one ohm across identical trace lengths.