Binary Phase
Intermetallic phases formed between gold surface finishes and tin-based solder alloys determine joint ductility during thermal aging. Gold-rich surface finishes exposed to molten tin solder dissolve rapidly to form gold-tin intermetallics, specifically the brittle ausn4 compound. This specific stoichiometry exhibits low fracture toughness compared to bulk solder or copper-tin intermetallics.
It forms predominantly at the interface between the substrate nickel layer and the bulk solder matrix during reflow soldering, depleting local tin and leaving voiding pathways.
Structural Failure
Solid-state growth of gold-tin intermetallic structures continues under operating conditions whenever assemblies endure elevated temperatures. Liquid tin dissolves gold plating almost instantly at standard reflow temperatures, migrating away from the substrate interface to form dispersed ausn4 needles throughout the joint volume. Under mechanical shock or cyclic thermal stress, fracture paths propagate rapidly along the brittle grain boundaries of these large intermetallic crystals.
The resulting failure presents as a clean cleavage plane at the nickel-solder interface or through the center of the joint bulk. Joint strength degrades sharply after thermal cycling, producing catastrophic electrical opens.
Thickness Limit
Fabrication specifications limit electrolytic gold coating thickness to prevent excessive gold concentration in the reflow volume. Standard immersion gold coatings of 0.05 to 0.1 micrometers avoid excessive intermetallic formation, whereas thick gold plating exceeding 0.5 micrometers requires chemical stripping before soldering. Controlled gold thickness maintains joint shear strength across thermal storage testing.