Crystalline Structure
Elongated hexagonal crystals forming at the interface between copper pads and tin-based solder characterize a specific phase of metallurgical bonding. These cu6sn5 intermetallic needles typically grow during the initial wetting process or through subsequent thermal aging as copper atoms diffuse into the tin matrix. While a thin layer of intermetallic compound is necessary for a strong electrical and mechanical connection, excessive needle growth can lead to embrittlement of the solder joint.
This phase appears most prominently in lead-free alloys such as SAC305 during the cooling stage of reflow.
Morphological Development
Rapid cooling suppresses the transition of these structures into a coarse morphology, whereas slow cooling encourages the formation of large, dendritic shapes. Large cu6sn5 intermetallic needles can bridge across the solder bulk, creating paths for crack propagation under mechanical stress. Trace additions of elements like nickel or cobalt are often used to modify the grain structure and prevent the needles from becoming too large.
Controlling the peak temperature and the duration of the liquid phase limits the volume of copper that dissolves into the solder. The dissolution rate determines the eventual density and length of the resulting crystals.
Failure Mode
Cross-sectional microscopy reveals the presence of these structures when examining joints that have failed under vibration or thermal shock. Excessive needle density at the interface reduces the ductility of the bond.