Stack Architecture
Thin-film metallic layers sputtered onto integrated circuit contact pads create a solderable interface while forming a diffusion barrier against liquid tin. Applying flip chip metallization involves depositing sequential thin films of titanium, nickel-vanadium, and copper over aluminum pad metallization. Titanium acts as an adhesion layer to the pad aluminum and passivation dielectric, while nickel-vanadium functions as the primary barrier against tin migration.
Copper forms the top wettable layer that reacts with molten solder to establish structural intermetallic bonds during reflow.
Diffusion Prevention
Deposition thickness of each barrier layer determines long-term solder joint stability during high-temperature storage and field operation. Thermal reflow dissolves the surface copper layer into molten lead-free solder, forming copper-tin intermetallic compounds such as Cu6Sn5 at the interface. Excessive reflow time or elevated temperatures consume the underlying nickel-vanadium layer, exposing titanium to tin and causing complete adhesion loss.
Vacuum sputtering chambers maintain background pressure below one microtorr to prevent layer oxidation during multi-target deposition steps. Thin spots or pinholes inside the barrier layer allow rapid tin diffusion toward aluminum, causing intermetallic voids and eventual pad cratering under mechanical vibration.
Shear Strength
Solder bump shear testing evaluates interfacial strength between the under-bump stack and substrate pads following thermal aging. Fracture modes transitioning from bulk solder shear to interface failure indicate metal layer degradation or incomplete intermetallic formation.