Thermal Aging Effects on Electroless Nickel Immersion Gold Interfaces
Electroless nickel immersion gold joints undergo rapid thermal aging degradation through nickel-phosphide segregation and Kirkendall voiding at elevated temperatures.

Electroless nickel immersion gold joints undergo rapid thermal aging degradation through nickel-phosphide segregation and Kirkendall voiding at elevated temperatures.