Chemical Affinity
Intermolecular forces arising from permanent dipoles and hydrogen bonding constitute the specific portion of a material’s surface energy that drives interaction with polar liquids. Measuring polar surface energy indicates the density of active chemical sites available for bonding on a circuit board or component. This value is calculated by subtracting the dispersive component from the total measured surface energy.
Component Influence
Surface treatments like plasma etching or corona discharge are primarily used to increase this specific energy component by adding oxygen-rich functional groups. Highly polar surfaces attract water and other polar solvents, resulting in low contact angles and efficient wetting. If the polar energy is too low, solder masks and conformal coatings may bead up or peel away after curing.
Achieving a balance between polar and dispersive forces is necessary for optimizing the performance of structural adhesives.
Coating Success
Printed electronics and additive manufacturing rely on high polar energy to ensure the stability of deposited conductive inks. When the polar contribution is well matched to the surface tension of the ink, the resulting traces exhibit sharp edges and uniform thickness. Contaminants such as silicone oils or mold release agents drastically reduce the polar energy and lead to adhesion failure.
Monitoring this property during production provides a reliable way to verify the cleanliness of the incoming substrates.