Gold Embrittlement Thresholds in Nickel Intermetallic Layers under High-Temperature Long-Term Storage Conditions
Immersion gold above 0.15 microns combined with high storage heat causes brittle intermetallic failure from gold concentrations exceeding three weight percent.