Air Extraction
Lamination processes use heat and pressure to bond together the multiple layers of a circuit board. Implementing vacuum lamination press cycles begins with drawing a deep vacuum in the chamber before the mechanical plates apply physical pressure. This step removes trapped air and moisture from the board layup, which prevents internal voids from forming during the resin cure.
Without this initial vacuum phase, the resin would trap pocketed gases that cause delamination during soldering.
Material Consolidation
Mechanical pressure and temperature rise are applied once the vacuum has cleared the gas pathways. During vacuum lamination press cycles, the temperature is ramped up to melt the resin, while the mechanical platens compress the layers together. This action encapsulates the copper traces and cures the prepreg to form a solid, rigid board.
This thermal phase must be controlled to prevent the resin from running out of the panel borders.
Process Profile
Multi-layer boards with high circuit densities require precise lamination programs to ensure reliable layer bonding. These programs must be tuned for the specific prepreg resin and copper weight used in the stack. Correct execution of these vacuum lamination press cycles results in consistent dielectric spacing and reliable signal lines.