Fabric Thickness
Standard woven electrical laminate designates 2116 glass style by a nominal cloth weight of one hundred eight grams per square meter and a finished resin cured thickness near zero point one millimeters. Multilayer printed circuit board fabrication relies on this specific reinforcement weave to balance dielectric spacing against internal plane separation during high pressure hydraulic lamination cycles. Resin flow characteristics during pressing depend heavily on yarn count and aperture size within the woven matrix.
Openings in the fabric allow epoxy matrix materials to bridge adjacent internal copper traces without creating dry spots or resin starved pockets. Fabricators select this particular style when inner layer copper weights demand moderate resin volume to fill etched copper valleys completely. Shear forces generated during subsequent routing and drilling operations test the mechanical stability of the resulting composite panel.
Resin Content
Prepreg suppliers treat the woven glass fabric with partially cured epoxy systems that yield a total resin weight fraction near fifty four percent. Dielectric constant values and dissipation factors derive directly from the ratio of glass fiber to cured resin in the finished composite layer. Thermal expansion coefficients along the X and Y axes remain tightly constrained by the woven quartz filaments while the Z axis expands proportionally to the resin volume fraction.
Excess resin creates dimensional instability during thermal excursions while insufficient resin leaves internal glass bundles exposed to moisture ingress and electrical shorting. Automated optical inspection systems mounted after the inner layer press cycle verify that the resin distribution remains uniform across the entire panel surface.
Trace Impedance
Controlled impedance calculations for high speed digital transmission lines incorporate the thickness and dielectric properties associated with 2116 glass style dielectrics. Signal propagation speeds fluctuate when local glass bundles shift beneath microstrip or stripline copper traces during multilayer lamination. Impedance testing coupons positioned on the panel borders undergo time domain reflectometry to confirm that finished trace dimensions meet specified electrical tolerances.
Signal integrity engineers specify this exact glass style to maintain target characteristic impedance values without forcing excessive dielectric stackup thicknesses. Dielectric breakdown voltage thresholds scale directly with the resin rich layers encapsulating the woven reinforcement.