Quantifying Non Linear Viscoelastic Rheology and Interfacial Shear Failure in Sequential HDI Core Stackups
Sequential HDI lamination traps viscoelastic shear stress at smooth foil interfaces, driving target pad delamination unless reflow dwell and pad anchors are pinned.