Corrosion Mechanism
Electrochemical pitting and dissolution of copper circuitry or tin-lead solder joints occur when ionic chloride or bromide residues break down natural surface passivation layers in the presence of adsorbed water. Accelerating halide attack drives an autocatalytic pitting cycle wherein small halide anions penetrate fractured oxide skins and establish localized anode cells. The reaction forms soluble metal-halide complexes, which subsequently hydrolyze to regenerate the original halogen ions and release free hydronium ions.
This regenerative loop preserves the corrosive species at the reaction front while deepening microscopic pits along conductor boundaries. The process is bounded by moisture availability, becoming dormant below twenty percent relative humidity where moisture monolayers fail to bridge adjacent conductors.
Electrochemical Propagation
Applied voltage bias across closely spaced traces accelerates the migration of halogen anions toward positively charged anode traces. Copper dissolves rapidly into cuprous ions, reacting with chloride to generate unstable cuprous chloride compounds. Subsequent moisture migration oxidizes these products into insoluble oxychlorides and hydrochloric acid, fueling dendritic filament growth across glass-epoxy interfaces.
Dendrite shorting causes catastrophic intermittent leakage currents during functional testing.
Cleanliness Threshold
Ion chromatography analysis quantifying ionic contamination per IPC-TM-650 Method 2.3.28 defines the boundary of surface cleanliness on assembled printed wiring boards. Total chloride equivalence must remain below predetermined limits, often set at 0.65 micrograms per square centimeter for high-reliability electronics. Visual inspection rarely identifies microscopic pitting until dendritic filaments or green copper corrosion bloom across solder masks.