Surface Interaction
The physical action of a liquid alloy spreading across and adhering to a metallic surface describes molten solder wetting during the assembly stage. This molten solder wetting depends on the reduction of surface tension by the flux and the cleanliness of the underlying copper or plating. A successful interaction results in a low contact angle where the solder feathers out to a thin edge.
The process is complete when the intermetallic bond is established and the solder begins to solidify upon cooling.
Acceptance Standard
Visual inspection according to IPC-A-610 verifies the quality of the bond by checking the wetting angle and the coverage area. When molten solder wetting is insufficient, the solder beads up into spheres or fails to cover the pad, a condition known as non-wetting or de-wetting. These failures often stem from oxidation on the pads or exhausted flux that can no longer remove surface contaminants.
Proper storage of boards and components prevents these defects by limiting exposure to humidity and oxygen. Quality depends on surface preparation.
Chemical Mechanism
Flux removes oxides from the metal surfaces and prevents new ones from forming while the heat is applied. This cleaning allows the atoms of the solder and the base metal to share electrons and form a permanent bond. The speed of this reaction determines the throughput of the production line.