Oxide Removal
Cleaning steps that strip the naturally occurring oxide layer from a metal surface are a prerequisite for creating a reliable metallurgical bond. In manufacturing, native oxide dissolution typically involves the use of acidic flux components that react with the oxides of copper or tin. This cleaning step must be completed during the initial stage of the reflow cycle to ensure the solder can wet the pad.
Flux Activity
Temperature serves as the primary driver for the speed and thoroughness of the cleaning process. As the assembly heats up, the activators in the flux become more aggressive, speeding up the rate of native oxide dissolution until the metal is exposed. A successful reaction leaves behind a clean, high-energy surface that is ready for the molten solder to spread.
If the flux is too weak or the oxide is too thick from improper storage, the dissolution will be incomplete. This failure leads to non-wetting or weak joints that may fail during subsequent thermal stress.
Reaction Product
Metal salts and water are the typical by-products formed when the acid reacts with the surface oxides. These residues must be either encapsulated by the remaining flux or washed away during a cleaning step to prevent future corrosion. The window for native oxide dissolution is limited by the evaporation of the flux solvent and the eventual charring of the active ingredients.