Phase Expansion
Deviating from simple parabolic rates, the expansion of chemical compounds at the solder pad interface follows complex time and temperature dependencies. The occurrence of non-linear intermetallic growth is often seen in systems where multiple phases like Cu6Sn5 and Cu3Sn develop simultaneously. These layers do not grow at the same speed, and their relative thicknesses change as the reaction progresses.
This complexity makes it difficult to predict the total thickness using basic square root of time equations.
Time Relation
Initial reaction rates are typically governed by the chemical reaction at the interface while later stages are limited by the diffusion of atoms through the existing layer. During non-linear intermetallic growth, the rate may slow down or accelerate depending on the grain structure of the intermetallic itself. Voids that form within the layer can also impede the movement of atoms, leading to a staggered growth pattern.
This behavior is most pronounced in modern lead free alloys containing small amounts of nickel or bismuth. The presence of impurities or trace elements in the plating can further complicate the kinetics by poisoning the growth sites. This leads to a layered structure that lacks the predictable properties of a standard binary system.
Interface Integrity
Structural stability of the solder joint is compromised when the growth of these brittle layers becomes excessive or uneven. Because non-linear intermetallic growth creates a non-uniform boundary, it can introduce localized stress points. These points are often where cracks begin when the assembly is subjected to thermal or mechanical strain.
Monitoring this growth through cross sectional analysis is a standard part of reliability testing for new material sets.