Lattice Reorientation
Plastic deformation during copper wire bonding and heavy wire wedge bonding forces crystal lattices to tilt internally through subgrain boundary rotation. Mechanical stress introduces dislocations that migrate into low energy dislocation walls, fragmenting the original crystal into distinct domains separated by low angle boundaries. Incremental misorientation accumulates under continuous ultrasonic scrub and thermocompression force, rotating these adjacent subgrains relative to one another.
Automated optical inspection systems fail to detect internal lattice tilt because surface appearance remains intact after bonding.
Interconnect Stability
Electrical resistance increases when cumulative misorientation exceeds specific angular thresholds within the deformed volume. Current crowding occurs at localized dislocation pile ups, generating excessive Joule heating during power cycling tests. Elevated temperature accelerates void formation along the newly rotated boundaries, leading eventually to open circuit failures in automotive power modules.
Destructive cross sectioning followed by electron backscatter diffraction reveals the true angular distribution across the deformed interface.
Process Verification
Shear testing measures bond strength indirectly by applying lateral force until the interconnect fractures. High misorientation angles correlate with reduced fracture energy and brittle failure modes during destructive pull testing. Process engineers adjust ultrasonic power and applied force profiles to restrict excessive lattice tilting during initial wedge placement.
Controlled deformation parameters limit subgrain rotation, ensuring long term reliability under extreme operational vibration.