Titanium Stannide Deposition
Titanium stannide layers form on copper interconnect pads through intermetallic growth during solder reflow cycles. TiSn2 establishes a stable diffusion barrier that prevents excessive copper consumption by molten tin. Liquid solder wets the titanium surface until atomic diffusion nucleates the intermetallic compound along the grain boundaries.
Solder joint reliability depends on controlling the thickness of this reaction layer during thermal aging. Excessive growth brittleness fractures the joint under mechanical stress.
Intermetallic Compound Growth
Diffusion kinetics govern the growth rate of the titanium stannide phase during high temperature exposure. Solid state reactions proceed when thermal energy drives tin atoms into the titanium lattice at the interface. Microstructural voids develop when vacancy condensation outpaces atomic replacement within the reaction zone.
X-ray diffraction analysis confirms the stoichiometric ratio of the crystalline lattice. Shear testing measures the mechanical strength of assemblies containing the intermetallic layer.
Thermal Stress Fracture
Cyclic temperature variations induce shear forces across the boundary between the copper pad and the intermetallic compound. Differential thermal expansion rates generate plastic deformation within the surrounding solder matrix. Microscopic cracks propagate along the titanium stannide interface when mechanical loads exceed the fracture toughness of the crystal structure.
Automated optical inspection fails to detect subsurface cleavage because the defect initiates entirely beneath the solder fillet. Scanning electron microscopy resolves the fracture surface morphology after destructive shear testing.