Mechanical Evaluation
Solder joint assessment methods apply tensile force to individual solder spheres to measure their mechanical attachment strength. Utilizing cold bump pull testing provides a quantitative assessment of the board level reliability of ball grid array packages. The instrument grips a single solder ball and pulls it vertically until separation occurs.
This test evaluates the strength of the bond between the solder and the metal pad.
Failure Analysis
Fracture surface analysis identifies the weakest interface in a solder connection after mechanical load application. During a cold bump pull sequence, the resulting fracture surface is inspected to locate traces of intermetallic compounds or pad cratering. High force values correspond to ductile failures within the solder alloy itself.
Low force values indicate brittle interfacial failures that point to problematic surface finishes or contamination during assembly. This analysis is performed using high magnification scanning electron microscopy to identify the specific failure region.
Adhesive Strength
Testing equipment utilizes specialized jaw assemblies to secure the solder sphere without inducing premature deformation before the pull force begins. Implementing the cold bump pull method requires precise alignment of the clamping tool with the vertical axis of the solder bump. The pull speed is controlled to ensure consistent stress distribution.