Electrochemical Process
Printed circuit board manufacturing relies on the deposition of a continuous metal layer within drilled through-holes to establish vertical electrical interconnects. This procedure, known as copper barrel electroplating, utilizes an acid copper bath to build up the thickness of copper on the hole walls to a specified dimension. The thickness must be sufficient to withstand the thermal expansion of the surrounding resin during assembly soldering.
A typical standard requires a minimum of twenty-five micrometers of plated copper inside each barrel.
Thermal Endurance
During solder reflow, the laminate material expands along its vertical axis at a rate much higher than that of the copper cylinder. Proper copper barrel electroplating ensures that the plated tube possesses both the thickness and the elongation properties needed to survive this stress without fracturing. If the plating is too thin or brittle, the barrel can develop circumferential cracks that cause intermittent or permanent circuit open failures.
Regular tensile strength and elongation tests of the copper deposit prevent such structural failures.
Plating Quality
Cross-sectioning and microscopic measurement of finished holes confirm that the deposit is uniform and free of voids. If the copper barrel electroplating fails to meet the thickness threshold, the entire panel is rejected before component mounting.