Gas Entrapment
Internal cavities formed within solder spheres represent a common discontinuity found in high-density surface mount packages with ball pitches below 0.5 millimeters. Occurrences of micro bga voiding are typically categorized by their size and location within the joint, particularly near the interface of the component pad and the solder ball. These air pockets are often invisible to the naked eye and require x-ray inspection to identify.
High levels of this defect can reduce the effective conductive area and create stress concentrators that lead to premature fatigue cracks.
Defect Formation
Evolution of flux volatiles during the reflow process remains the primary driver of this phenomenon. When micro bga voiding occurs, it is frequently because the entrapped gas cannot escape through the molten solder before the joint solidifies. This is exacerbated by smaller ball diameters which offer a shorter path for gas movement but have a high surface-to-volume ratio that increases the likelihood of flux entrapment.
Solder paste chemistry and the specific reflow profile soak time also influence the final volume of gas trapped within the sphere.
Inspection Acceptance
Manufacturing standards such as IPC-A-610 define the maximum allowable area of a void as a percentage of the total ball image. While micro bga voiding is often permitted up to twenty-five percent of the ball area, some high-reliability applications demand even lower thresholds. Exceeding these limits necessitates rework or scrapping of the assembly.