Molecular Migration
Movement of polymer chains across the interface of two distinct prepreg or core layers during the lamination process creates a unified structural bond. Resin cross-diffusion occurs when the heat and pressure of the press cycle reduce the viscosity of the resin, allowing it to flow and intermingle at the microscopic level. This process is the primary mechanism for the mechanical adhesion between the layers of a multilayer circuit board.
Interfacial Strength
Achieving a high degree of diffusion is necessary to prevent delamination during the thermal stress of soldering or environmental cycling. If the resin reaches its gel point too quickly, the lack of sufficient diffusion results in a weak bond that is susceptible to separation. Factors such as the ramp rate of the press temperature and the age of the prepreg material influence the window of time during which resin cross-diffusion can effectively occur.
Successful diffusion results in a homogenous boundary that distributes mechanical stress evenly throughout the stackup.
Chemical Compatibility
When using different resin systems in a hybrid stackup, the resins must be chemically compatible to allow for effective cross-diffusion. Incompatible materials will fail to bond correctly, leading to voids or immediate failure upon cooling.