Laminate Defect
Internal material separation describes an area in a woven glass laminate where the resin has failed to fill the spaces between the warp and fill yarns. A resin window void typically occurs during the lamination process if the prepreg has insufficient resin content or the press cycle temperature is incorrect. This defect appears as a clear, unfilled opening in the weave when viewed under transmitted light.
IPC standards classify these voids as major or minor defects depending on their size and proximity to conductive patterns.
Process Origin
Inadequate laminate flow or excessive heat rise during the early stages of pressing can cause the epoxy to cure before it wets all fiber bundles. This premature curing results in the formation of a resin window void in areas of high fabric tension. Precise ramp rates and vacuum assistance during lamination minimize the occurrence of these dry spots.
Reliability Effect
Moisture accumulation in these unfilled areas can lead to electrical failure when the printed circuit board is placed in a humid environment. The resin window void creates a path where copper can migrate or where conductive anodic filaments can grow between adjacent plated through-holes. Furthermore, trapped air inside the void expands rapidly during lead-free reflow soldering, causing localized delamination or blisters that ruin the assembly.
This expansion also puts stress on nearby solder joints, increasing the risk of mechanical cracks during thermal cycles.