Metallurgical Dissolution
Dissolution of plated hole metallization during contact with molten solder reduces the structural thickness of conductive through-hole barrels in printed circuit assemblies. Wave soldering and automated selective soldering expose barrel walls to molten tin alloys, frequently causing sleeve erosion at the hole entrance and along thin plating zones. Tin-rich lead-free solders actively dissolve copper metallization when dwell times or pot temperatures exceed standard operating envelopes.
The defect appears as thinned or completely missing copper along the knee and barrel walls of the plated hole. Assemblies with initial plating thicknesses near lower specification limits prove especially vulnerable to complete sleeve dissolution.
Thermal Exposure
Extended contact duration with liquid solder waves above two hundred sixty degrees Celsius accelerates metal dissolution rates. Multiple rework passes compound initial copper loss by repeatedly exposing fragile barrel walls to fresh flux and molten alloy.
Workmanship Limit
Microsection evaluations performed per IPC-TM-650 Method 2.1.1 determine remaining copper barrel thickness following soldering operations. Inspection criteria under IPC-6012 and IPC-A-610 mandate that sleeve erosion must not reduce the remaining copper wall thickness below the minimum specified plating threshold, typically eighteen micrometers for Class 3 performance. Severe erosion severing the connection between the internal trace and the through-hole barrel causes catastrophic open circuits under thermal cycling.
Selective solder process controls limit dwell times to three seconds or less to preserve sleeve integrity on heavy backplane boards. Quality departments reject completed lots whenever cross-sectional analysis reveals copper sleeve breaching or annular ring detachment caused by excessive solder contact.