Quantifying Thermally Activated Intermetallic Growth in Micro-BGA Solder Joints
Quantifying micro-BGA intermetallic growth requires measuring initial reflow layer thickness and calculating Arrhenius diffusion rates to avoid boundary voiding.

Quantifying micro-BGA intermetallic growth requires measuring initial reflow layer thickness and calculating Arrhenius diffusion rates to avoid boundary voiding.

Repeated reflow passes accelerate interfacial Cu6Sn5 and Cu3Sn growth, exhausting solder compliance and driving brittle fracture under thermomechanical stress.

Solid state intermetallic growth degrades lead-free solder joints through parabolic Cu3Sn layer thickening and Kirkendall void embrittlement under thermal aging.