Corrosive Action
Solder fluxes designed for wave and reflow soldering operations utilize organic acids to remove metal oxides and promote wetting of the solder alloy. Undesired organic acid flux erosion occurs when active residues remain on the printed circuit board after soldering and attack the metal features. This reaction gradually dissolves the copper traces and exposed solder pads, leading to open circuits.
Cleanliness standards require the total removal of these aggressive compounds before the boards are packaged.
Process Vulnerability
High-temperature exposure activates the acid components, but if the temperature or time is insufficient during reflow, the flux may not fully decompose or volatilize. Under these conditions, the organic acid flux erosion is accelerated by the presence of residual humidity on the board surface. The corrosion is particularly severe on fine-pitch components where small spaces trap the liquid flux residues.
Solder joints exposed to these residues can degrade within days of manufacture. Processing engineers adjust the wash cycle temperature and water pressure to ensure that no active residue remains in these tight spaces.
Mitigation Technique
Removing flux residues involves high-pressure wash systems and deionized water. Post-wash resistivity measurements confirm that organic acid flux erosion has been prevented by removing the conductive contaminants. If ionic contamination levels exceed the specified limit, the boards are recycled through the wash.
This continuous verification maintains the long-term reliability of the circuitry.